PROPERTIES THAT MATTER
- Mold Density: 0.3 g/cm³ (Method ISO 845: 2009-10)
- Hardness Shore A: 40 (Method ISO 868: 2003)
- Tensile Strength: 3 N/mm² (Method ISO 22654: 2002)
- Elongation at Break: 280% (Method ISO 22654: 2002)
- Tear Strength: 4 N/mm (Method ISO 20872: 2001)
- Split Tear: 2.6 N/mm (Method ASTM D 3574 Test F)
- Retention of Tensile Strength after 7 Days Hydrolysis, 70°C,
100 RH%: > 90% (Method ISO 22654: 2002)